Hot patch vs cold patch on my cracked apron, cold won by a mile
Last fall I filled a 4 foot crack near the street with hot patch from a bag I warmed up, but it crumbled out by March. This spring I tried the cold patch in the bucket, packed it down with a 2x4 and some gravel dust, and it's still holding after a heavy rain. The hot stuff felt like it never bonded to the edges, just sat there like a loose tooth. Anyone else have better luck with one over the other, or am I missing something about how to prep the crack?
Check the temp of the mix before you blame the product, because hot patch from a bag only works if it is still soft enough to actually mold into the crack walls. If it cooled on the ride home or sat in the truck bed too long, it skins over and just plugs the hole instead of fusing, which is exactly why yours popped out like a loose tooth. Cold patch gets a bad name mostly from people who skip the gravel dust or tamp it in too thin, and it sounds like you nailed the two things that matter.