Used to grind welds with a flap disc until my helper said the panel looked like a golf ball
Back in 2019 I was finishing every quarter panel with a 40 grit flap disc and calling it good, which worked fine until a customer at my shop here in Tulsa pointed out the waves under his fresh paint. Switched to a 3 inch roloc with 80 grit and a light hand after that, and the filler work stopped fighting me. What grit are you all running on your final pass before primer?